Optimum alloy compositions in reduced-activation martensitic 9Cr steels for fusion reactor
- 1 October 1992
- journal article
- Published by Elsevier in Journal of Nuclear Materials
- Vol. 195 (1-2) , 51-67
- https://doi.org/10.1016/0022-3115(92)90363-p
Abstract
No abstract availableKeywords
This publication has 28 references indexed in Scilit:
- Development of potential low activation ferritic and austenitic steelsPublished by Elsevier ,2003
- Impact behavior of reduced-activation ferritic steels irradiated in the Fast Flux Test FacilityJournal of Nuclear Materials, 1992
- Tensile properties of 9Cr-1MoVNb and 12Cr-1MoVW steels irradiated to 23 dpa at 390 to 550 ° CJournal of Nuclear Materials, 1991
- Mechanical property changes and microstructures of iron irradiated with fission and fusion neutronsJournal of Nuclear Materials, 1991
- Irradiation hardening and ductility loss of a low-activation 9Cr-1V ferritic steel at low temperaturesJournal of Nuclear Materials, 1989
- Phase stability of reduced activation ferritic steel: 8%Cr-2%W-0.2%V-0.04%Ta-FeJournal of Nuclear Materials, 1988
- Materials selection for reduced activation of fusion reactorsJournal of Nuclear Materials, 1988
- Microstructure and toughness of Cr-W and Cr-V ferritic steelsJournal of Nuclear Materials, 1988
- Effect of specimen size on the ductile-brittle transition behavior and the fracture sequence of 9Cr-W steelsJournal of Nuclear Materials, 1987
- Effects of irradiation on low activation ferritic alloysJournal of Nuclear Materials, 1987