Laser-Raman Spectroscopic Study of the Adhesive Interface Between 4-MET/MMA-TBB Resin and Hydroxyapatite or Bovine Enamel
- 1 January 1991
- journal article
- Published by Japanese Society for Dental Materials and Devices in Dental Materials Journal
- Vol. 10 (2) , 105-120,231
- https://doi.org/10.4012/dmj.10.105
Abstract
The possible chemical interaction between synthetic hydroxyapatite or bovine enamel and a functional monomer of 4-methacryloxyethyl trimellitic acid (4-MET) diluted in methyl methacrylate (MMA) was examined by measuring the Raman spectra. It was concluded that the carboxyl group of 4-MET reacted with the calcium in the substrate to form a salt that was detected by the Raman band at around 1, 380cm-1. However, formation of the salt on the surface of the hydroxyapatite (HAP) with the carboxyl group, and polymerization of the 4-MET in the methacryl group near the surface were mutually exclusive reactions for the same 4-MET molecule.Keywords