New aspects in cationization of lignocellulose materials. I. Preparation of lignocellulose materials containing quarternary ammonium groups
- 1 February 1984
- journal article
- research article
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 29 (2) , 637-642
- https://doi.org/10.1002/app.1984.070290219
Abstract
TMAHP derivatives were prepared by the reaction of beech sawdust with CHMAC in alkaline medium. The examination of the reaction conditions showed that the most suitable molar ratio was NaOH/CHMAC = 1.8 (1 ml 17.5% NaOH/1 mL 50% CHMAC). At this ratio the maximum degree of substitution expressed by the exchange capacity of 0.35 mmol/g of modified sawdust was obtained by using 1.5–2mL of 50% aqueous solution of CHMAC/g sawdust. The optimal reaction time at 60°C was 2 h. This condition gave yields of modified sawdust above 90% and soluble derivatives mainly consisting of hemicelluloses up to 12%.Keywords
This publication has 2 references indexed in Scilit:
- Review of Drug-free therapeutic community: An evaluation.Contemporary Psychology, 1980
- Wood Hemicelluloses: Part IPublished by Elsevier ,1964