Fabrication of low-loss and wide-bandwidth v.a.d. optical fibres at 1.3 μm wavelength

Abstract
A low-loss and wide-bandwidth optical fibre in the long-wavelength region has been fabricated by the v.a.d. method. Loss at 1.3 μm is 0.98 dB/km and 6 dB down bandwidth is 1600 MHz km at 1.26 μm.