Abstract
Titanium oxide nanotubes were fabricated by anodic oxidation of a pure titanium sheet in an aqueous solution containing 0.5 to 3.5 wt% hydrofluoric acid. These tubes are well aligned and organized into high-density uniform arrays. While the tops of the tubes are open, the bottoms of the tubes are closed, forming a barrier layer structure similar to that of porous alumina. The average tube diameter, ranging in size from 25 to 65 nm, was found to increase with increasing anodizing voltage, while the length of the tube was found independent of anodization time. A possible growth mechanism is presented.Keywords
This publication has 8 references indexed in Scilit:
- Magnetoelastic sensors in combination with nanometer-scale honeycombed thin film ceramic TiO2 for remote query measurement of humidityJournal of Applied Physics, 2000
- Formation of Porous TiO2 by Anodic Oxidation and Chemical Etching of TitaniumElectrochemistry, 2000
- Self-ordered pore structure of anodized aluminum on silicon and pattern transferApplied Physics Letters, 2000
- Surface micropatterning to regulate cell functionsBiomaterials, 1999
- Self-organized formation of hexagonal pore arrays in anodic aluminaApplied Physics Letters, 1998
- Photocatalytic decomposition of NO at 275 K on titanium oxide catalysts anchored within zeolite cavities and frameworkApplied Surface Science, 1997
- Solid‐State Gas Sensors: A ReviewJournal of the Electrochemical Society, 1992
- Nucleation and growth of porous anodic films on aluminiumNature, 1978