Preparation of high-modulus and high-strength nylon-6 fibre by the zone-annealing method
- 31 July 1982
- Vol. 23 (8) , 1193-1198
- https://doi.org/10.1016/0032-3861(82)90378-0
Abstract
No abstract availableKeywords
This publication has 15 references indexed in Scilit:
- Mechanical properties and superstructure of high‐modulus and high‐strength PET fiber prepared by zone annealingJournal of Applied Polymer Science, 1981
- Preparation of high-modulus and high-strength poly(ethylene terephthalate) fiber by zone annealingJournal of Applied Polymer Science, 1981
- Recent developments in ultraorientation of polyethylene by solid-state extrusionChemical Reviews, 1980
- Preparation of High Modulus and High Strength Fiber by Zone-annealing MethodSen'i Gakkaishi, 1980
- Urinary tract infection in newborn.BMJ, 1972
- Effect of orientation, anisotropy, and water on the relaxation behavior of nylon 6 from 4.2 to 300°KJournal of Polymer Science Part A-2: Polymer Physics, 1972
- Mechanical relaxations in polyamidesJournal of Polymer Science Part A-2: Polymer Physics, 1971
- Bond rupture in highly oriented crystalline polymersJournal of Polymer Science Part A-2: Polymer Physics, 1969
- The crystal structure of polycaproamide: Nylon 6Journal of Polymer Science, 1955
- The Relation of Dielectric Properties to Structure of Crystalline Polymers. II. Linear PolyamidesJournal of the American Chemical Society, 1942