Effect of microstructure and hydrides on fracture of TiAl
- 1 September 1991
- journal article
- Published by Elsevier in Scripta Metallurgica et Materialia
- Vol. 25 (9) , 2133-2138
- https://doi.org/10.1016/0956-716x(91)90287-b
Abstract
No abstract availableThis publication has 14 references indexed in Scilit:
- An elastic-plastic stress analysis for a notched bar in plane strain bendingPublished by Elsevier ,2002
- Effects of grain size on yield strength in TiAlScripta Metallurgica et Materialia, 1991
- Intermetallic Compounds for Strong High-Temperature Materials: Status and PotentialAnnual Review of Materials Science, 1989
- The high temperature α field in the titanium-aluminum phase diagramScripta Metallurgica, 1988
- Bend tests and fracture mechanism of TiAl single crystals at 293–1073 KActa Metallurgica, 1988
- Yielding and work hardening effects in notched bend barsJournal of the Mechanics and Physics of Solids, 1986
- Hydrogen-assisted fracture at notchesMaterials Science and Technology, 1985
- Roughness-Induced Crack Closure: An Explanation for Microstructurally Sensitive Fatigue Crack GrowthMetallurgical Transactions A, 1983
- Fatigue deformation of TiAl base alloysMetallurgical Transactions A, 1977
- The deformation and fracture of TiAl at elevated temperaturesMetallurgical Transactions A, 1975