Abstract
The dielectric loss tangent of yttria stabilised zirconia (YSZ) was measured at approximately 5.5 GHz using the dielectric rod resonator method (DRRM). The measured values of tan δ were 9 × 10−4 at 300 K and 3 × 10−4 at 77 K.