The structural relaxation behavior of Pd48Ni32P20, Fe75Si10B15 and Co72.5Si12.5B15 amorphous alloy wire and ribbon
- 31 October 1983
- journal article
- Published by Elsevier in Scripta Metallurgica
- Vol. 17 (10) , 1205-1208
- https://doi.org/10.1016/0036-9748(83)90284-3
Abstract
No abstract availableKeywords
This publication has 7 references indexed in Scilit:
- Production of amorphous CoSiB and CoMSiB (M ≡ Group IV – VIII transition metals) wires by a method employing melt spinning into rotating water and some properties of the wiresMaterials Science and Engineering, 1982
- Mechanical properties of Fe-Si-B amorphous wires produced by in-rotating-water spinning methodMetallurgical Transactions A, 1982
- Production of Fe-P-C amorphous wires by in-rotating-water spinning method and mechanical properties of the wiresJournal of Materials Science, 1982
- The critical thickness for the formation of Ni-Si-B amorphous alloysMetallurgical Transactions A, 1981
- Production of PdCuSi amorphous wires by melt spinning method using rotating waterScripta Metallurgica, 1981
- Production of Metal Filament by In-Rotating-Water Spinning MethodJournal of the Japan Institute of Metals and Materials, 1981
- Structure relaxation spectrum of metallic glassesApplied Physics Letters, 1976