Abstract
High purity aluminum was anodized in sulfuric acid solutions at various concentrations (5– 50%), temperatures (10°– 50°C), time periods (2 – 60 min), and current densities (1.7 – 6.2 amp/dm2). The coating weight, metal loss, coating ratio, sealing weight gain, dyed color, density, and coating chemical dissolution rate were determined.