High performance 2:17 type SmCo permanent magnets with low temperature coefficients
- 3 November 1998
- journal article
- Published by Elsevier in Solid State Communications
- Vol. 108 (9) , 667-670
- https://doi.org/10.1016/s0038-1098(98)00441-4
Abstract
No abstract availableKeywords
This publication has 8 references indexed in Scilit:
- Domain wall pinning sites in Sm(CoFeCuZr) magnetsJournal of Magnetism and Magnetic Materials, 1997
- The effects of intrinsic coercivity on the thermal stability of Sm(Co0.70Fe0.21Cu0.06Zr0.03)7.6 sintered magnets up to 450 °CJournal of Applied Physics, 1997
- Domain-wall curvature and coercivity in pinning type Sm–Co magnetsJournal of Applied Physics, 1997
- Temperature Compensation in the '2:17' type magnetsIEEE Transactions on Magnetics, 1985
- Internal temperature compensation of rare earth-cobalt permanent magnets for microwave devices by adding heavy lanthanidesJournal of the Less Common Metals, 1983
- High coercive force 2–17type Sm1−xErx(Co0.69Fe0.22Cu0.08Zr0.02)7.22 magnets with a low temperature coefficientJournal of the Less Common Metals, 1983
- Magnetic domains in rare-earth cobalt permanent magnetsIEEE Transactions on Magnetics, 1982
- The 2-17 type Sm2-xHRExCo10Cu1.5Fe3.2Zr0.2(HRE=Gd, Tb, Dy, Ho, Er) magnets with low temperature coefficientIEEE Transactions on Magnetics, 1980