Elevated temperature combined erosion-corrosion of steels
- 15 July 1986
- Vol. 110 (2) , 117-149
- https://doi.org/10.1016/0043-1648(86)90142-0
Abstract
No abstract availableThis publication has 6 references indexed in Scilit:
- Oxide-formation characteristics in the early stages of oxidation of Fe and Fe-Cr alloysOxidation of Metals, 1983
- The Growth of Hematite Blades during the High Temperature Oxidation of IronMetallurgical Transactions A, 1982
- Erosion of elevated-temperature corrosion scales on metalsWear, 1981
- The corrosion of some superalloys in contact with coal chars in coal gasifier atmospheresOxidation of Metals, 1981
- Solid particle erosion mechanisms in copper and two copper alloysMetallurgical Transactions A, 1981
- Particulate erosion of NiO scalesWear, 1981