Determination of impurities in lead zirconate–titanate electroceramics by inductively coupled plasma atomic emission spectrometry
- 1 January 1992
- journal article
- research article
- Published by Royal Society of Chemistry (RSC) in Journal of Analytical Atomic Spectrometry
- Vol. 7 (6) , 877-882
- https://doi.org/10.1039/ja9920700877
Abstract
An analytical method was developed for the determination of Al, Ba, Ca, Hf, Mg, Si and Sr impurities and Co, Cr, Cu, Fe, Mn, Nb, Ni, P, W and Zn dopants in lead zirconate–titanate (PZT) electroceramics by inductively coupled plasma atomic emission spectrometry. A niobium-doped dense PZT ceramic sample was used. Sample dissolution was achieved by using: decomposition with HF + H2SO4 in a poly(tetrafluoroethylene)-lined pressure vessel at 170 °C for 16 h followed by evaporation to dryness and dissolution of the residue with HCl; decomposition with (NH4)2SO4+H2SO4 in a glass beaker followed by evaporation to dryness and dissolution of the residue with HCl; and fusion with Li2B4O7 in a graphite crucible and dissolution of the melt with 1+24 v/v HNO3. For each element, an analytical line free from spectral interference was selected. The decomposition reagents present in the final solutions of the sample (HCl and Li2B4O7–HNO3), and the Ti and Zr macro-constituents, decrease the emission signals substantially. Nevertheless, the inter-element effect of Pb is negligible. The correction of these matrix effects was carried out by preparing standard solutions, for obtaining detection limits, and calibration by matrix matching. The 3σ detection limits of the impurities were determined using the three decomposition methods and correction of the matrix effects. The lowest values of the detection limits were obtained using acid decompositions, and were between ≈0.1 µg g–1 for CaO, MgO and SrO, and 461 µg g–1 for P2O5. The analytical results obtained for 17 minor and trace elements using the three decomposition methods were in excellent agreement. Good precision and accuracy were attained; the relative standard deviations for the results obtained for each element for each dissolution method ranged in general from 3 to 7%.Keywords
This publication has 16 references indexed in Scilit:
- Determination of phosphorus in zircons by inductively coupled plasma atomic emission spectrometryAnalytical Chemistry, 1989
- Chemical analysis by inductively coupled plasma atomic emission spectrometry of semiconducting ceramics of barium titanate doped with various metal oxidesMicrochimica Acta, 1989
- Effect of dopants on the microstructure and lattice parameters of lead zirconate-titanate ceramicsJournal of Materials Science, 1987
- Atomic Emission Sources for Solution SpectrochemistryAnalytical Chemistry, 1986
- Analytical inductively coupled plasma spectroscopies — past, present, and futureAnalytical and Bioanalytical Chemistry, 1986
- Effect of simultaneous heterovalent substitutions on both cationic sites on the electrical conductivity and ageing of PZT type ceramicsFerroelectrics, 1983
- Effects of impurity doping in lead zirconate-titanate ceramicsFerroelectrics, 1982
- Lead Zirconate‐Lead Titanate Piezoelectric Ceramics with Iron Oxide AdditionsJournal of the American Ceramic Society, 1969
- Electromechanical Properties of Lead Titanate Zirconate Ceramics with Lead Partially Replaced by Calcium or StrontiumJournal of the American Ceramic Society, 1959
- Piezoelectric Properties of Lead Zirconate-Lead Titanate Solid-Solution CeramicsJournal of Applied Physics, 1954