Development of the microhardness of an al‐2.0 at.% zn‐1.3 at.% mg alloy with additions of technical impurities during a two‐step ageing treatment (ii)
- 1 January 1982
- journal article
- Published by Wiley in Crystal Research and Technology
- Vol. 17 (2) , 267-273
- https://doi.org/10.1002/crat.2170170222
Abstract
No abstract availableKeywords
This publication has 4 references indexed in Scilit:
- Isothermal Ageing in the T Range from 0°C to 180°C of a Technical Al‐2.0 at.% Zn‐1.3 at.% Mg Alloy after Direct QuenchCrystal Research and Technology, 1982
- On the precipitation of n′ phase in an AlZnMg alloyScripta Metallurgica, 1978
- On the position of the coherency spinodal curve in an Al-Zn (18 at.%) alloyCrystal Research and Technology, 1977
- A transmission electron microscopy investigation of the early stages of precipitation in an Al-Zn-Mg alloyMetallurgical Transactions A, 1976