Cavitation and cracking in as-cast and superplastic Pb-Sn eutectic during high-temperature fatigue
- 1 May 1987
- journal article
- research article
- Published by Springer Nature in Journal of Materials Science Letters
- Vol. 6 (5) , 549-551
- https://doi.org/10.1007/bf01739280
Abstract
No abstract availableKeywords
This publication has 15 references indexed in Scilit:
- Cavitation in high purity aluminium during fatigue at elevated temperaturesJournal of Materials Science Letters, 1983
- Simple reverse bending machine for low cycle fatigue at elevated temperaturesReview of Scientific Instruments, 1983
- The role of Coble creep and interface control in superplastic Sn-Pb alloysJournal of Materials Science, 1983
- Fracture of a tin-lead eutectic alloy in Region III of superplastic flowJournal of Materials Science, 1982
- Experimental constitutive relations for the high temperature deformation of a PbSn eutectic alloyMaterials Science and Engineering, 1981
- HVEM observations of grain boundary voids in high purity copperActa Metallurgica, 1981
- An investigation of intercrystalline and interphase boundary sliding in the superplastic Pb-62% Sn eutecticActa Metallurgica, 1979
- Superplastic deformation, cavitation, and fracture of microduplex Cu-Ni-Zn alloysMetallurgical Transactions A, 1978
- Superplastic deformation of the Pb-Sn eutecticJournal of Materials Science, 1976
- Creep behaviour in the superplastic Pb–62% Sn eutecticPhilosophical Magazine, 1975