Abstract
Narayanaswamy's model of structural relaxation has been shown to provide an excellent description of the behavior of a variety of glasses. In the standard formulation, the relaxation time, τ is represented by the Arrhenius equation, with the activation energy partitioned between the temperature and Active temperature. That form for τ is successful, but lacks theoretical justification. In this paper, the Adam‐Gibbs equation is shown to describe accurately both τ and the viscosity of NBS 710 (alkali lime silicate) glass. This equation is expected to be accurate over a wider range of temperature and Active temperature than the Arrhenius equation.