Picosecond optical studies of amorphous diamond and diamondlike carbon: Thermal conductivity and longitudinal sound velocity
- 1 September 1994
- journal article
- research article
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 76 (5) , 2636-2640
- https://doi.org/10.1063/1.357560
Abstract
A picosecond pump‐probe technique is used to measure the room‐temperature thermal conductivity κ and longitudinal sound velocity cl of amorphous diamond (a‐D) and diamondlike carbon (DLC) thin films. Both κ and cl were found to decrease with film hydrogen content. Depending on the film deposition technique, κ is in the range 5–10×10−2 W cm−1 K−1 for a‐D, and 3–10×10−3 W cm−1 K−1 for DLC. Values of cl were found to be in the range 14–18×105 cm s−1 for a‐D, and 6–9×105 cm s−1 for DLC.This publication has 24 references indexed in Scilit:
- Heat flow and lattice vibrations in glassesPublished by Elsevier ,2002
- Stresses in diamond-like carbon filmsDiamond and Related Materials, 1993
- Glasslike thermal transport in heavily irradiated diamondPhysical Review B, 1993
- Measurements of the Kapitza conductance between diamond and several metalsPhysical Review Letters, 1992
- Compressive-stress-induced formation of thin-film tetrahedral amorphous carbonPhysical Review Letters, 1991
- Ion-beam sputtered diamond-like carbon with densities of 2.9 g/ccJournal of Vacuum Science & Technology A, 1991
- Characterization of diamondlike carbon films and their application as overcoats on thin-film media for magnetic recordingJournal of Vacuum Science & Technology A, 1987
- Ion beam deposition of special film structuresJournal of Vacuum Science and Technology, 1981
- Preparation of hard coatings by ion beam methodsThin Solid Films, 1979
- The thermal conductivity of dielectric crystals: the effect of isotopesProceedings of the Royal Society of London. Series A. Mathematical and Physical Sciences, 1956