The effect of surface pre-treatment on carbon solution and deposition in the iron-methane reaction
- 31 December 1977
- Vol. 15 (4) , 205-210
- https://doi.org/10.1016/0008-6223(77)90001-x
Abstract
No abstract availableKeywords
This publication has 11 references indexed in Scilit:
- Impurity deposition from an evaporated solvent and its effect on steel oxidationJournal of Chemical Technology & Biotechnology, 1976
- The production and properties of filamentous carbonCarbon, 1975
- Kinetics of the deposition of pyrolytic carbon on nickelCarbon, 1975
- Graphite formation by the dissolution—precipitation of carbon in cobalt, nickel and ironCarbon, 1975
- Formation of carbonaceous deposits from the reaction of methane over nickelCarbon, 1975
- Carbon formation on iron and nickel foils by hydrocarbon pyrolysis—reactions at 700°CCarbon, 1974
- Growth of filamentary carbon on metallic surfaces during the pyrolysis of methane and acetoneCarbon, 1973
- Carbon formation from methane pyrolysis over some transition metal surfaces—II. Manner of carbon and graphite formationCarbon, 1972
- Carbon formation from methane pyrolysis over some transition metal surfaces—I. Nature and properties of the carbons formedCarbon, 1970
- Growth of single-crystal graphite by pyrolysis of acetylene over metalsCarbon, 1969