Energy requirements for the size reduction of poplar and aspen wood
- 10 January 1989
- journal article
- research article
- Published by Wiley in Biotechnology & Bioengineering
- Vol. 33 (2) , 207-210
- https://doi.org/10.1002/bit.260330210
Abstract
The energy requirements associated with conventional mechanical size reduction of poplar and aspen wood are compared to a new method of size reduction employing a wood planer. Although the planer requires about 2.3 times less energy to achieve the same size reduction as conventional methods, large-scale equipment to implement this approach does not currently exist. Explosive depressurization was also compared to conventional mechanical size reduction. The conventional mechanical methods require roughly 70% more energy to achieve the same size reduction as explosive depressurization. Thus, explosive depressurization appears to be the preferred method and has the added benefit of altering the chemical structure of the wood to enhance the enzymatic hydrolysis of the cellulose fraction.This publication has 6 references indexed in Scilit:
- Steam‐explosion pretreatment of wood: Effect of chip size, acid, moisture content and pressure dropBiotechnology & Bioengineering, 1986
- Alkali‐explosion pretreatment of straw and bagasse for enzymic hydrolysisBiotechnology & Bioengineering, 1986
- Enzymic saccharification of pretreated wheat strawBiotechnology & Bioengineering, 1985
- Enzymic saccharification of sugarcane bagasse pretreated by autohydrolysis–steam explosionBiotechnology & Bioengineering, 1983
- Enzyme management in the iotech processBiotechnology & Bioengineering, 1983
- Enzymatic hydrolysis of cellulose and various pretreated wood fractionsBiotechnology & Bioengineering, 1982