Electrodeposition of Rhodium and Ruthenium for Slip-ring Surfaces
- 1 January 1965
- journal article
- research article
- Published by Taylor & Francis in Transactions of the IMF
- Vol. 43 (1) , 135-142
- https://doi.org/10.1080/00202967.1965.11869966
Abstract
The mechanical wear of rhodium and ruthenium electrodeposits operating as slip-ring surfaces with palladium-silver alloy brushes is shown to be a function of electrolyte composition, plating conditions, and thickness of coating. Within selected thickness ranges the deposits function very satisfactorily and are resistant to wear. Types of roughness which should be avoided are discussed, and methods of measuring and controlling these are recommended. It is concluded that for slip-rings a thickness of 40 x 10−6 in should be sufficient to withstand the conditions involved in the majority of applications, and that for such duty ruthenium provides a more suitable surface than rhodium.Keywords
This publication has 7 references indexed in Scilit:
- Surface films on precious-metal contactsBritish Journal of Applied Physics, 1962
- Properties and Behaviour of Precious-Metal Electrodeposits for Electrical ContactsTransactions of the IMF, 1962
- Relation of Temperature to Quantity of Forage Consumed by Chickens on RangePoultry Science, 1961
- Electrodeposition of RutheniumTransactions of the IMF, 1961
- Instrument for the measurement of specular reflectivity of bright metal surfacesJournal of Scientific Instruments, 1960
- Some Experimental Observations on the Effect of Addition Agents on Stress and Cracking in Rhodium DepositsTransactions of the IMF, 1959
- Some Experimental and Practical Aspects of Heavy Rhodium PlatingTransactions of the IMF, 1955