Fatigue of unidirectional SCS-6/Ti-24Al-11Nb composite containing a circular hole
- 1 July 1994
- journal article
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 25 (7) , 1413-1424
- https://doi.org/10.1007/bf02665474
Abstract
No abstract availableKeywords
This publication has 6 references indexed in Scilit:
- Crack initiation around holes in a unidirectional MMC under fatigue loadingEngineering Fracture Mechanics, 1992
- Elevated temperature fatigue behavior of SCS-6/Ti24Al11NbMaterials Science and Engineering: A, 1992
- Effect of environment on the thermal fatigue response of an SCS-6/Ti-24Al-11Nb compositeMetallurgical Transactions A, 1992
- Prediction of Matrix Fatigue Crack Initiation in Notched SCS-6/Ti-15-3 Metal Matrix CompositesJournal of Composites Technology and Research, 1992
- Thermal fatigue of Ti-24Ai-11NB/SCS-6Metallurgical Transactions A, 1990
- Damage Initiation and Growth in Fiber Reinforced Metal Matrix CompositesPublished by ASTM International ,1989