Induced and spontaneous strain in ferroelectric ferroelastic tanane
- 1 January 1976
- journal article
- research article
- Published by Taylor & Francis in Ferroelectrics
- Vol. 13 (1) , 319-321
- https://doi.org/10.1080/00150197608236599
Abstract
Physical properties of the organic material tanane1 do not allow sufficiently accurate polarization measurements. As an alternative, the following order parameters were studied: spontaneous shear strain x 6, (linearly coupled to spontaneous polarization P 3), and spontaneous birefringence Δn 6, shown to be proportional to the spontaneous strain. Results of induced birefringence and strain, above and below the transition temperature (Tc = 13.5°C), are reported and discussed.Keywords