Identification of the Initial Oxide Films on 18-8 Stainless Steel in High Temperature Water
- 1 October 1968
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 24 (10) , 336-337
- https://doi.org/10.5006/0010-9312-24.10.336
Abstract
Initial oxide film formed on 18–8 stainless steel in high temperature water at 300 C (572 F) for 1 hour was identical with corundum type crystals like (Cr, Fe)2O3 alone or its coexistence with α-Fe2O3. On the contrary, the oxide film produced by prolonged oxidation (24 hours) consisted mainly of the spinel type crystals containing nickel.Keywords