Studies of the chemical degradation of polysiloxanes by hydrofluoric acid: 1. Poly (tetramethyl-p-silphenylene siloxane)
- 31 December 1976
- Vol. 17 (12) , 1086-1090
- https://doi.org/10.1016/0032-3861(76)90010-0
Abstract
No abstract availableKeywords
This publication has 21 references indexed in Scilit:
- A study of the fold surface structure of polyethylene single crystals by means of selective degradation with ozoneJournal of Polymer Science: Polymer Physics Edition, 1975
- The morphology of ultradrawn polyethylene. I. Nitric acid etching plus gel permeation chromatographyJournal of Polymer Science: Polymer Physics Edition, 1975
- Gel‐permeation chromatographic studies of cellulose degradation. III. Methanolysis of celluloseJournal of Polymer Science: Polymer Physics Edition, 1974
- Morphology of siloxane block copolymers: Tetramethyl‐p‐silphenylene siloxane–dimethylsiloxaneJournal of Polymer Science: Polymer Physics Edition, 1974
- Influence of morphology on the transport properties of crystalline polymersPublished by Walter de Gruyter GmbH ,1974
- Thermal degradation of nylon 66Journal of Polymer Science Part A-1: Polymer Chemistry, 1971
- Abbau von aus der schmelze kristallisiertem polyäthylen durch salpetersäureDie Makromolekulare Chemie, 1968
- Infrared studies of chain folding in polymers. II. Polyethylene terephthalateJournal of Macromolecular Science, Part B, 1967
- Heat content of amorphous regions of drawn linear polyethylneJournal of Polymer Science Part B: Polymer Letters, 1965
- Selective oxidation with nitric acid reveals the microstructure of polypropyleneJournal of Polymer Science Part B: Polymer Letters, 1965