Deactivation of supported metal catalysts by carbon or coke formation is a problem of serious magnitude in steam reforming, methanation, and other important catalytic processes. Its causes are generally threefold: (1) fouling of the metal surface, (2) blockage of catalysts pores and voids, and/or (3) actual physical disintegration of the catalyst support. Since loss of catalytic activity and physical destruction of the catalyst by carbon deposits can occur rapidly (within hours or days) under unfavorable conditions, understanding and control of these effects are of major technological and economical importance.Keywords
This publication has 73 references indexed in Scilit:
- Hydrogenation of surface carbon on alumina-supported nickelJournal of Catalysis, 1979
- Mechanism of carbon formation during steamcracking of hydrocarbonsCarbon, 1977
- AES end LEED evidence for dicarbon fragments on Ni(110)Journal of Catalysis, 1977
- Mechanisms of carbon formation on nickel-containing catalystsJournal of Catalysis, 1977
- The Formation and Removal of Coke from Nickel CatalystCatalysis Reviews, 1977
- Abstract: Adsorption and decomposition of ethylene on Ni(110)Journal of Vacuum Science and Technology, 1977
- A study of the kinetics and mechanism of the decomposition of formic acid on carburized and graphitized Ni(110) using AES, LEED and flash desorptionJournal of Catalysis, 1975
- The poisoning of a steam hydrocarbon gasification catalystJournal of Catalysis, 1972
- Commentaires sur “Auger spectroscopy of carbon on Ni” De J. P. Coad et J. C. RivièreSurface Science, 1971
- Auger spectroscopy of carbon on nickelSurface Science, 1971