Elastic, piezoelectric, and dielectric properties of the BaLaGa3O7 crystal
- 15 September 1985
- journal article
- research article
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 58 (6) , 2285-2287
- https://doi.org/10.1063/1.335947
Abstract
The elastic, piezoelectric, and dielectric constants of single‐crystal BaLaGa3O7, which belongs to the 4̄2m class of the tetragonal system, were measured. The six independent elastic constants, two piezoelectric constants, and coupling coefficients were determined using standard resonance‐antiresonance measurements and the following results were received (cij in 1011 N/m2): c11=1.78, c12=1.03, c33=1.17, c13=0.88, c44=0.39, c66=0.54, e14=0.29 C/m2, e36=0.10 C/m2, kl14=0.141, and kl36=0.055. The two dielectric constants were measured at low frequency using a three electrode configuration. The relative values of these constants were determined to be εT11/ε0=12.7, εS11/ε0=12.4, εT33/ε0=9.5, εS33/ε0=9.5.This publication has 2 references indexed in Scilit:
- Linear Theory of PiezoelectricityIEEE Transactions on Sonics and Ultrasonics, 1984
- Absorption and birefrigence of BaLaGa3O7 single crystalsPhysica B+C, 1984