Investigation of LaNi5 after prolonged cycling
- 1 January 1991
- journal article
- Published by Elsevier in Journal of the Less Common Metals
- Vol. 172-174, 997-1008
- https://doi.org/10.1016/s0022-5088(06)80005-6
Abstract
No abstract availableKeywords
This publication has 22 references indexed in Scilit:
- Degradation processes in a LaNi5 electrodeJournal of the Less Common Metals, 1989
- Kinetic measurements of LaNi5Hx and MmNi4.15 Fe0.85Hx with constant pressure differentialsJournal of the Less Common Metals, 1989
- Modifications near the surface owing to hydrogen cycling of the intermetallics LaNi5 and LaNi5−xAlxJournal of the Less Common Metals, 1987
- The accommodation of strain and particle size broadening in rietveld refinement; its application to de-deuterided LaNi5 alloyJournal of the Less Common Metals, 1987
- Effects of lattice strain on the hysteresis of pressure-composition isotherms for the LaNi5H2 systemJournal of the Less Common Metals, 1985
- Cyclic life of metal hydrides with impure hydrogen: Overview and engineering considerationsJournal of the Less Common Metals, 1984
- Stability of rechargeable hydriding alloys during extended cyclingJournal of the Less Common Metals, 1984
- Life properties of TiMn alloy hydrides and their hydrogen purification effectJournal of the Less Common Metals, 1983
- Cycling hydriding response of LaNi5 in hydrogen containing oxygen as a minor impurityJournal of the Less Common Metals, 1983
- Degradation of Lani5 hydrogen-absorbing material by cyclingJournal of the Less Common Metals, 1980