PREPARATION OF SEMICONDUCTING CERAMICS (NTC THERMISTORS) BY CHEMICAL METHOD

Abstract
The decomposition in controlled atmosphere of mixed oxalic precursors (Mn1-yNiy)C2O4, 2H 2O allows at low temperature (600-700°C), direct preparation of powders of nickel manganites Mn3-xNixO4(