High temperature corrosion behavior of iron aluminides containing ternary additions in H2/H2S/H2O mixed gases
- 31 December 1997
- journal article
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 239-240, 859-870
- https://doi.org/10.1016/s0921-5093(97)00676-x
Abstract
No abstract availableKeywords
This publication has 11 references indexed in Scilit:
- The corrosion behavior of Fe-Al alloys in H2/H2S/H2O atmospheres at 700–900°COxidation of Metals, 1997
- The high-temperature corrosion behavior of Fe-Mo-Al alloys in H2/H2O/H2S mixed-gas environmentsOxidation of Metals, 1993
- A comprehensive investigation of the sulfidation behavior of binary Co-Mo alloysOxidation of Metals, 1990
- Transport properties of sulfide scales and sulfidation of metals and alloysOxidation of Metals, 1985
- Application of Wagner's Theory to the Parabolic Growth of Oxides Containing Different Kinds of Defects: II . Doped OxidesJournal of the Electrochemical Society, 1981
- The thermochemistry of transition metal sulfidesOxidation of Metals, 1977
- The scaling behavior of an iron-5% aluminum alloy in sulfur vaporOxidation of Metals, 1969
- Kinetics, Microstructures and Mechanism of Internal Oxidation - Its Effect and Prevention in High Temperature Alloy OxidationCorrosion, 1965
- The Oxidation off Iron, Nickel and Cobalt-Base Alloys Containing AluminumCorrosion, 1965
- Passivity and inhibition during the oxidation of metals at elevated temperaturesCorrosion Science, 1965