Application of an asymmetrical four point bend shear test to solder joints
- 1 September 2001
- journal article
- research article
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 30 (9) , 1206-1213
- https://doi.org/10.1007/s11664-001-0151-7
Abstract
No abstract availableKeywords
This publication has 12 references indexed in Scilit:
- A shear test method to measure shear strength of metallic materials and solder joints using small specimensScripta Materialia, 1999
- A Test Method to Measure Shear Strength of Ceramic Joints at High TemperaturesJournal of the American Ceramic Society, 1997
- Stress relaxation behavior of eutectic tin-lead solderJournal of Electronic Materials, 1995
- Converting to lead-free solders: An automotive industry perspectiveJOM, 1993
- Further development of the losipescu shear test methodExperimental Mechanics, 1987
- Investigation of the superplasticity of tin-lead eutectic by impression creep testsJournal of Materials Science, 1986
- Microstructural Observations and Mechanical Behavior of Pb-Sn Solder on Copper PlatesMRS Proceedings, 1986
- The losipescu shear test as applied to composite materialsExperimental Mechanics, 1983
- Stress relaxation in Tin-Lead soldersMaterials Science and Engineering, 1979
- Experimental determination of stiffness properties of thin-shell composite cylindersExperimental Mechanics, 1966